Alternate Names: Frit 110, Frit GF110
Description: Zinc sodium frit for textured tile glazes
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 4.20% | 0.18 | |
| Na2O | 9.40% | 0.36 | |
| ZnO | 15.50% | 0.46 | |
| B2O3 | 30.20% | 1.04 | |
| SiO2 | 40.70% | 1.62 | |
| Oxide Weight | 239.87 | ||
| Formula Weight | 239.87 | ||
| Materials |
Pemco Frit P-1733
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Fusion Frit FZ-16
The champion in our frit melt-off competitition. This frit showcases the amazing fluxing power of boron and zinc working together. It is 15.5% ZnO. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.90 |
|---|---|
| Frit Softening Point | 1450F |