Description: Mystery frit without exact chemistry
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Li2O | 2.50% | 0.26 | .5 |
| Na2O | 6.50% | 0.32 | 2.5 |
| K2O | 2.50% | 0.08 | 1.5 |
| CaO | 4.50% | 0.24 | 1.5 |
| ZnO | 1.50% | 0.06 | 1.5 |
| SrO | 1.50% | 0.04 | 1.5 |
| Al2O3 | 12.50% | 0.37 | 2.5 |
| B2O3 | 12.50% | 0.55 | 2.5 |
| SiO2 | 55.00% | 2.79 | 5 |
| Oxide Weight | 301.47 | ||
| Formula Weight | 301.47 | ||
We only have ranges for the chemistry on this material.
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.2 |
|---|---|
| Frit Softening Point | 1350C |