Alternate Names: Fusion Frit FZ576
Description: Ca-Zn transparent monoporosa frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZnO | 11.80% | 0.34 | |
| CaO | 10.00% | 0.42 | |
| Na2O | 5.00% | 0.19 | |
| K2O | 2.10% | 0.05 | |
| Al2O3 | 5.80% | 0.13 | |
| B2O3 | 4.30% | 0.14 | |
| SiO2 | 61.00% | 2.38 | |
| Oxide Weight | 234.66 | ||
| Formula Weight | 234.66 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.2 x 10-6 |
|---|---|
| Frit Softening Point | 1800F |