Alternate Names: Frit FZ276
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 5.85% | 0.49 | |
| K2O | 0.14% | 0.01 | |
| Na2O | 5.85% | 0.44 | |
| ZnO | 1.00% | 0.06 | |
| ZrO2 | 8.65% | 0.33 | |
| B2O3 | 12.00% | 0.81 | |
| Al2O3 | 7.10% | 0.33 | |
| SiO2 | 59.41% | 4.65 | |
| Oxide Weight | 470.80 | ||
| Formula Weight | 470.80 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3336
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |