Fusion Frit F-95

Alternate Names: Fusion Frit F95

Description: Opacified flux for wall tile

Oxide Analysis Formula Tolerance
BaO 0.50% 0.01
CaO 4.00% 0.28
K2O 2.50% 0.10
Na2O 9.50% 0.60
ZrO2 17.20% 0.55
B2O3 17.50% 0.99
Al2O3 7.00% 0.27
SiO2 41.50% 2.72
Oxide Weight 392.01
Formula Weight 392.01

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Frit 282-b
Materials Hommel Frit 477
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.35 x 10-6
Frit Softening Point 1500F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy