Description: Reimbold & Strick fast firing Zn,Ba matte frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 3.00% | 0.12 | |
| K2O | 1.00% | 0.02 | |
| ZrO2 | 11.00% | 0.20 | |
| Na2O | 3.00% | 0.11 | |
| MgO | 1.00% | 0.06 | |
| BaO | 18.00% | 0.27 | |
| ZnO | 15.00% | 0.42 | |
| Al2O3 | 7.00% | 0.16 | |
| B2O3 | 5.00% | 0.16 | |
| SiO2 | 36.00% | 1.36 | |
| Oxide Weight | 227.80 | ||
| Formula Weight | 227.80 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 56 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | 660C |
| Glass Transition Temperature | 600C |