Description: Barium manganese borosilicate low alumina frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZnO | 3.70% | 0.16 | |
| Na2O | 2.80% | 0.16 | |
| Li2O | 1.40% | 0.17 | |
| MnO2 | 15.90% | 0.66 | |
| CaO | 2.60% | 0.17 | |
| BaO | 14.10% | 0.33 | |
| SiO2 | 35.70% | 2.15 | |
| Al2O3 | 4.70% | 0.17 | |
| B2O3 | 19.10% | 0.99 | |
| Oxide Weight | 362.43 | ||
| Formula Weight | 362.43 | ||
Unknown European supplier
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |