Fiber

Description: POLYOLEGIN FIBER, NYLON, HERCULON

Notes

Short cut straight fibers are valuable when used as a clay mix additive (.1-.5%) to greatly increase green strength and drying performance. Fiber is typically used in heavy clay products, such as refractories, where considerable internal stresses are developed during drying. These fibers burn out during firing and have little or no impact on the strength of the fired product.

One problem with the use of fiber additives in clay bodies is that it becomes difficult to cut the plastic material with a wire or knife because the fiber wraps around the leading edge in an increasingly thicker layer, as it is pulled through the clay. In addition, fiber additions are not suitable for items that will need to be trimmed in the leather hard state.

It can be difficult to disperse the clumped fibers evenly throughout a clay mix. One solution is to disperse them in very hot water first then add this to the clay mix.

Hercules company produces a wide variety of fiber products in different colors, lengths and densities for use in filtration, asphalt, concrete, etc. Those of most interest to the clay industry are:

Product Color Length Application

2.2 Den T-153 White 5mm, 10mm Wet Clay
3.0 Den T-153 White 3mm, 5mm, 10mm, 3/4" Wet Clay
4.0 Den T-157 Gray 10mm Asphalt
15.0 Den T-157 White 10mm Asphalt
3.0 Den T-158 White 3/4" Concrete
15.0 Den T-158 White 3/4", 1 1/2" Concrete

Hercules Inc.
Fibers Division
3169 Holcomb Bridge Road
Suite 700
Norcross, GA 30071-1394
404-447-9120 800-241-0340

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Additives for Ceramic Bodies
Materials that are added to bodies to impart physical working properties and usually burn away during firing. Binders enable bodies with very low or zero clay content to have plasticity and dry hardness, they can give powders flow properties during pressing and impart rheological properties to clay slurries. Among potters however, it is common for bodies to have zero additives.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy