Ferro Frit CM-943

Oxide Analysis Formula Tolerance
K2O 0.30% 0.01
Na2O 2.70% 0.13
PbO 43.50% 0.58
ZnO 7.60% 0.28
B2O3 5.00% 0.21
Al2O3 5.00% 0.15
SiO2 35.90% 1.78
Oxide Weight 298.51
Formula Weight 298.51

Notes

Yellow leadless cadmium, underglaze mix; complete by itself. Works well with CM-942 to produce oranges. Cone 06.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Available from Laguna Clays

Data

Frit Softening Point 1750F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy