Description: Australian equivalent of Frit 3134
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 20.10% | 0.68 | |
| Na2O | 10.30% | 0.32 | |
| B2O3 | 23.10% | 0.63 | |
| SiO2 | 46.50% | 1.48 | |
| Oxide Weight | 190.69 | ||
| Formula Weight | 190.69 | ||
Alumina free version of Frit 4108
| Materials |
Ferro Frit 3134
A frit with 23% B2O3. The most common of frits used in pottery in North America. Around the world, other companies make frits of equivalent chemistry. |
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 4108
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |