Ceradel Frit C 1249

Alternate Names: C1249 Fritte, C 1249 Fritte, Ceradel Frit 1249,C-1249

Description: Lead bisilicate frit, Bisilicate de plomb

Oxide Analysis Formula Tolerance
PbO 70.00% 1.00 20
SiO2 19.00% 1.01 10
B2O3 11.00% 0.50
Oxide Weight 318.86
Formula Weight 318.86

Notes

Similar to a lead bisilicate, but with significant boron.

We have another source that says this is just a lead bisilicate. So the analysis is uncertain.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Ceradel Frit C 1250
Materials Ceradel Frit C 1251
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.

Data

Co-efficient of Linear Expansion 85 (10-7/C 20/300C)
Frit Softening Point 600-700C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy