Description: Calcium Borate Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 27.10% | 1.00 | |
| B2O3 | 50.44% | 1.50 | |
| Al2O3 | 4.77% | 0.10 | |
| SiO2 | 17.68% | 0.61 | |
| Oxide Weight | 206.99 | ||
| Formula Weight | 206.99 | ||
A fritted substitute for colemanite.
CaO = 27.10
Al2O3 = 4.77
SiO2 = 17.68
B2O3 = 50.44
Firing Range 1030°C - 1180°C
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron). |
| Materials |
Colemanite
A natural source of boron that melts at a very low temperature. |
| Materials |
Turkish Colemanite
A mineral with very high B2O3 and CaO content. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk