Formula: Ca3(PO4)2
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 54.24% | 0.75 | |
| P2O5 | 45.76% | 0.25 | |
| Oxide Weight | 77.56 | ||
| Formula Weight | 77.56 | ||
| Materials |
Tricalcium Phosphate
|
| Materials |
Bone Ash
|
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Typecodes |
Opacifier
Opacifiers are powders that turn transparent glazes opaque by various chemical and physical mechanisms (and combinations of mechanisms). |
| Frit Softening Point | 1670C |
|---|