Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 61.50% | 4.16 | |
| Al2O3 | 25.10% | 1.00 | |
| Fe2O3 | 1.00% | 0.03 | |
| CaO | 0.06% | - | |
| MgO | 0.77% | 0.08 | |
| TiO2 | 1.27% | 0.06 | |
| Na2O | 0.16% | 0.01 | |
| K2O | 2.88% | 0.12 | |
| LOI | 7.29% | n/a | |
| Oxide Weight | 376.87 | ||
| Formula Weight | 406.51 | ||
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |
| Materials |
Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries. |
| URLs |
http://www.walkerceramics.com.au/Raw Mat'l typical_analysis.htm
Walker Ceramics materials |