Description: Tennessee Ball Clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.01 | |
| K2O | 0.30% | 0.01 | |
| MgO | 0.20% | 0.02 | |
| Na2O | 0.10% | - | |
| TiO2 | 2.20% | 0.08 | |
| Al2O3 | 33.20% | 1.00 | |
| SiO2 | 50.20% | 2.57 | |
| Fe2O3 | 1.00% | 0.02 | |
| LOI | 12.60% | n/a | |
| C | 0.30% | n/a | |
| Oxide Weight | 268.52 | ||
| Formula Weight | 308.29 | ||
Particle Size (e.s.d.)
125 microns - 0.2
20 microns - 96
2 microns - 78
Modulus of Rupture at 110C
Mn/M2 - 3.9
lbf/in2 - 560
Water Absorption
1120C - 16.0
1220C - 8.0
Shrinkage Dry to Fired
1120C - 4.0
1220C - 14.0
Refractoriness
Cone - 33, 1730C
| Materials |
Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries. |
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |