Pemco Frit P-930

Alternate Names: Frit 930, Frit P930

Description: Leadless all-fritted base

Oxide Analysis Formula Tolerance
CaO 5.40% 0.29
Na2O 4.30% 0.21
SrO 17.30% 0.50
ZrO2 1.20% 0.03
B2O3 15.40% 0.67
Al2O3 4.10% 0.12
SiO2 52.30% 2.62
Oxide Weight 300.66
Formula Weight 300.66

Notes

For cone 06-02, stronita replaces lead in Pb-742. Blends with P-786 for intermediate temperatures.

Related Information

Links

Materials Fusion Frit F-38
High strontium low alumina borosilicate flux.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.8 x 10-6 (50-450C)
Co-efficient of Linear Expansion 6.8
Frit Melting Range (C) 1500-1600F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy