March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.
| Monthly Tech-Tip | No tracking! No ads! No paywall! |
Alternate Names: Frit 926, Frit P926
Description: Leadless fast fire frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 17.00% | 0.68 | |
| K2O | 0.30% | 0.01 | |
| Na2O | 8.50% | 0.31 | |
| B2O3 | 18.70% | 0.61 | |
| Al2O3 | 5.00% | 0.11 | |
| SiO2 | 50.50% | 1.90 | |
| Oxide Weight | 225.57 | ||
| Formula Weight | 225.57 | ||
Replaced P-54 in wall tile industry. It has lower solubility to prevent thickening or 'set' in glaze slurries.
| Materials |
Ferro Frit 3288
|
| Materials |
Fusion Frit F-13
|
| Materials |
Pemco Frit P-1R63
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Pemco Frit P-54
|
| Materials |
General Frit GF-103
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.4 x 10-6 (50-450C) |
|---|---|
| Frit Melting Range (C) | 1650-1700F |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk