1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit P-786

Alternate Names: Frit 786, Frit P786

Description: Leadless all-fritted glaze

Oxide Analysis Formula Tolerance
CaO 11.50% 0.58
K2O 3.00% 0.09
Na2O 2.00% 0.09
SrO 8.70% 0.24
B2O3 8.80% 0.36
Al2O3 6.80% 0.19
SiO2 59.20% 2.79
Oxide Weight 283.23
Formula Weight 283.23

Notes

Used for vitreous and semi-vitreous dinnerwre and artware. Same as Pb-349 with strontia replacing lead. Fires cone 02-8.

Related Information

Links

Materials Pemco Frit Pb-349
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 630
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.2 x 10-6 (50-450C)
Frit Melting Range (C) 1640-1910F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy