Description: High expansion zirconia fluorine frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 4.80% | 0.25 | |
| Na2O | 13.40% | 0.63 | |
| ZnO | 3.40% | 0.12 | |
| ZrO2 | 13.10% | 0.31 | |
| B2O3 | 18.20% | 0.76 | |
| Al2O3 | 7.40% | 0.21 | |
| 2.40% | - | ||
| SiO2 | 27.40% | 1.33 | |
| F | 9.80% | 1.50 | |
| Oxide Weight | 283.88 | ||
| Formula Weight | 283.88 | ||
Used in satin matte crackle glazes at Cone 06
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 12.10 |
|---|---|
| Co-efficient of Linear Expansion | 12.10 (50-350C) |
| Frit Softening Point | 1300F |
| Frit Melting Range (C) | 1250-1350F |
| Co-efficient of Linear Expansion | 12.1x10-6 (50-350C) |
| I.F.P. (celsius) | 475C |