Fusion Frit FZ-430

Alternate Names: Fusion Frit FZ430

Description: Calcium zinc frit

Oxide Analysis Formula Tolerance
CaO 10.00% 0.59
K2O 2.00% 0.07
Na2O 4.00% 0.21
SrO 2.00% 0.06
ZnO 1.50% 0.06
B2O3 11.50% 0.55
Al2O3 10.50% 0.34
SiO2 58.50% 3.23
Oxide Weight 331.42
Formula Weight 331.42

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.45
Frit Softening Point 1500F
By Tony Hansen