April 2026: We are continuing a major code rewrite, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.

Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads! No paywall!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit FR-170A

Description: Opaque white glaze frit cone 06-04

Oxide Analysis Formula Tolerance
BaO 1.50% 0.06
CaO 0.60% 0.06
MgO 0.90% 0.13
Na2O 5.50% 0.51
PbO 7.00% 0.18
ZnO 1.00% 0.07
ZrO2 12.40% 0.57
B2O3 13.90% 1.14
Al2O3 5.70% 0.32
SiO2 51.50% 4.89
Oxide Weight 570.88
Formula Weight 570.88

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy