Alternate Names: Frit F380
Description: Barium leadless frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 18.50% | 0.40 | |
| CaO | 6.60% | 0.39 | |
| Na2O | 3.80% | 0.20 | |
| B2O3 | 8.50% | 0.41 | |
| Al2O3 | 6.00% | 0.20 | |
| SiO2 | 56.00% | 3.11 | |
| Oxide Weight | 331.76 | ||
| Formula Weight | 331.76 | ||

This picture has its own page with more detail, click here to see it.
Fired at 350F/hr to 1300F and held for 15 minutes. Some are still burning off carbon (which seems strange). There are two early leaders: Ferro frit 3110 and Fusion frit F75 are starting to deform (they have almost the same chemistry). Amazingly, these two frits have low boron, they rely on high soda as the flux.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |