1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-300

Alternate Names: Fusion Frit F300

Description: Strontium frit for sanitaryware

Oxide Analysis Formula Tolerance
CaO 10.00% 0.56
K2O 1.80% 0.06
Na2O 2.70% 0.14
SrO 8.20% 0.25
B2O3 5.00% 0.22
Al2O3 10.10% 0.31
SiO2 62.40% 3.24
Oxide Weight 313.07
Formula Weight 313.07

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-4K47
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.29
Frit Softening Point 1800F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy