April 2026: We are continuing a major code rewrite, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.
| Monthly Tech-Tip | No tracking! No ads! No paywall! |
Description: Leadless calcium borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 16.80% | 0.67 | |
| K2O | 0.40% | 0.01 | |
| Na2O | 8.70% | 0.32 | |
| B2O3 | 19.30% | 0.62 | |
| Al2O3 | 5.00% | 0.11 | |
| SiO2 | 49.80% | 1.87 | |
| Oxide Weight | 225.21 | ||
| Formula Weight | 225.21 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Fusion Frit F-13
|
| Materials |
Ferro Frit 3288
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.9 x 10-6 |
|---|---|
| Frit Melting Range (C) | 1500F |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk