| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.65% | 0.04 | |
| Na2O | 0.65% | 0.05 | |
| TiO2 | 0.40% | 0.03 | |
| Al2O3 | 20.00% | 1.00 | |
| SiO2 | 75.90% | 6.44 | |
| Fe2O3 | 0.40% | 0.01 | |
| LOI | 2.00% | n/a | |
| Oxide Weight | 499.80 | ||
| Formula Weight | 510.00 | ||
This version has lower alklai (and therefore higher PCE), finer particle size, lower specific gravity and bulk density.
| Materials |
Alkatrol W-20031
|
| Materials |
Alkatrol
|
| Typecodes |
Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate. |
| Pyrometric Cone Equivalent | 19 |
|---|