| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 1.30% | 0.07 | |
| Na2O | 1.30% | 0.10 | |
| TiO2 | 0.51% | 0.03 | |
| Al2O3 | 21.00% | 1.00 | |
| SiO2 | 73.09% | 5.91 | |
| Fe2O3 | 0.41% | 0.01 | |
| LOI | 2.40% | n/a | |
| Oxide Weight | 474.11 | ||
| Formula Weight | 485.76 | ||
This version has higher alklai (and therefore lower PCE), coarser particle size, higher specific gravity and bulk density.
| Materials |
Alkatrol W-22535
|
| Materials |
Alkatrol
|
| Typecodes |
Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate. |
| Pyrometric Cone Equivalent | 16 |
|---|