Esmalglass Frit FM 1403/G

Oxide Analysis Formula Tolerance
SiO2 53.00% 2.74
Na2O 1.20% 0.06
MgO 1.60% 0.12
BaO 0.50% 0.01
Fe2O3 0.10% -
K2O 5.40% 0.18
SrO 7.00% 0.21
Al2O3 21.00% 0.64
ZrO2 0.10% -
ZnO 2.70% 0.10
PbO 0.30% -
CaO 5.60% 0.31
LOI 0.60%n/a
Oxide Weight 306.33
Formula Weight 308.18

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 950C
Frit Melting Range (C) 1285C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy