1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Esmalglass Frit FO-961/P

Oxide Analysis Formula Tolerance
ZnO 13.30% 0.33
TiO2 0.10% -
Fe2O3 0.10% -
MgO 3.80% 0.19
Na2O 0.30% 0.01
Al2O3 5.20% 0.10
K2O 5.50% 0.12
SiO2 53.40% 1.81
ZrO2 7.40% 0.12
CaO 9.20% 0.33
P2O5 0.80% 0.01
LOI 0.60%n/a
Oxide Weight 202.02
Formula Weight 203.24

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 960C
Frit Melting Range (C) 1170C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy