Alternate Names: Fusion Frit F5
Description: Strontium Barium flux
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.22% | 0.49 | |
| BaO | 11.73% | 0.21 | |
| Na2O | 1.72% | 0.07 | |
| K2O | 2.42% | 0.07 | |
| SrO | 6.04% | 0.16 | |
| Al2O3 | 5.14% | 0.14 | |
| B2O3 | 6.12% | 0.24 | |
| SiO2 | 56.62% | 2.54 | |
| Oxide Weight | 269.99 | ||
| Formula Weight | 269.99 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.13 x 10-6 |
|---|---|
| Frit Softening Point | 1800F |