1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Glasurfritten 35.2

Alternate Names: 35 2,35-2

Description: Bleihaltige Zinkmatt-Fritte

Oxide Analysis Formula Tolerance
PbO 23.00% 0.19
CaO 5.00% 0.16
Na2O 2.00% 0.06
ZnO 27.00% 0.60
B2O3 4.00% 0.10
Al2O3 2.00% 0.04
SiO2 37.00% 1.11
Oxide Weight 179.82
Formula Weight 179.82

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 61 x 10-7
Frit Softening Point 600C
Frit Melting Range (C) 970-1030C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy