Frit A 3128

Description: Reimbold & Strick stoneware BaO, CaO, zinc matte frit

Oxide Analysis Formula Tolerance
ZnO 30.00% 0.51
Na2O 8.00% 0.18
Al2O3 3.00% 0.04
CaO 10.00% 0.24
BaO 8.00% 0.07
B2O3 5.00% 0.10
SiO2 36.00% 0.82
Oxide Weight 137.36
Formula Weight 137.36

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 74 x 10-7 (20-400C)
Frit Softening Point 610C
Glass Transition Temperature 560C