G-200 EU Feldspar

Description: G200 equivalent from Spain

Oxide Analysis Formula Tolerance
SiO2 68.50% 7.06
Al2O3 17.00% 1.03
Fe2O3 0.10% -
TiO2 0.03% -
K2O 11.00% 0.72
Na2O 2.10% 0.21
CaO 0.50% 0.06
MgO 0.08% 0.01
LOI 0.50%n/a
Oxide Weight 614.76
Formula Weight 617.85

Notes

This is being sold by Imerys as an equivalent to G200 Feldspar (because the mine of the latter was closed in 2013 because the deposit was depleted). The data sheet says it is obtained from a feldspathic sand by a flotation process.

It is 70% K Feldspar, 23% Na Feldspar, 7% quartz.

Particle size:
+200 mesh: 0.5%
+325 mesh: 6.2%

On paper, the chemistry is pretty similar to G-200.
Laguna Clay is now selling Mahavir Feldspar from India as the G200 equivalent.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
Materials G-200 Feldspar
Materials G200 Old Blend Feldspar
Materials Mahavir Potash Feldspar
Materials G-200 2R Feldspar
URLs https://digitalfire.com/4sight/datasheets/G-200-EU.pdf
G-200-EU Datasheet

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy