Fayles Blue Ball

Alternate Names: Fayles Blue Ball Clay

Description: Ball Clay

Oxide Analysis Formula Tolerance
CaO 0.23% 0.01
K2O 2.90% 0.10
MgO 0.77% 0.06
Na2O 0.89% 0.05
TiO2 1.00% 0.04
Al2O3 31.00% 1.00
SiO2 52.00% 2.85
Fe2O3 1.40% 0.03
LOI 9.20%n/a
Oxide Weight 296.75
Formula Weight 326.82

Notes

Particle Size (e.s.d.)
5 microns - 96
2 microns - 88
1 microns - 79
0.5 microns - 62
0.1 microns - 14

Rational Analysis (mica convention)
Clay 44%
Micaceous matter 35%
Quartz 15%

Modulus of Rupture at 100C
kgf/cm2 - 80.9

Refractoriness
PCEe - 32-33

Related Information

Links

Materials Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries.
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy