Zettlitzer Kaolin

Alternate Names: Sedlecký Kaolin

Oxide Analysis Formula Tolerance
CaO 0.14% 0.01
Al2O3 39.36% 1.00
SiO2 46.27% 2.00
Fe2O3 0.74% 0.01
LOI 13.00%n/a
Oxide Weight 224.19
Formula Weight 257.69

Notes

Sedlec la is the most well-known and oldest product made by Sedlecký Kaolin (Czech Republic). It has been produced since 1892, when Zettlitzer Kaolinwerke AG was founded. Today’s Sedlecký Kaolin is its successor.

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
Typecodes Materials used in Denmark

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy