Alternate Names: Icecap K
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 51.70% | 2.03 | 0.7 |
| Al2O3 | 43.20% | 1.00 | 1.0 |
| Fe2O3 | 0.20% | - | |
| TiO2 | 2.00% | 0.06 | 0.5 |
| LOI | 0.50% | n/a | |
| Oxide Weight | 229.26 | ||
| Formula Weight | 230.42 | ||
Conventionally calcined kaolin.
Burgess Icecap K, Iceberg and No. 30 calcined kaolins differ slightly in the pH, brightness, #325 residue, % free moisture. None of the differences should have significant effects on ceramic glaze and body applications.
However their Optiwhite thermo optic kaolins have the same chemistry but have an amorphous particle shape and lower specific gravity.
| Materials |
Calcined Kaolin
This is kaolin powder that has been fired in a furnace to remove the 12% crystal water and render it non-plastic. |
| URLs |
http://burgesspigment.com/BurgessWebsite.nsf/ICEBERG.pdf?OpenFileResource
Iceberg Kaolin Datasheet |
| URLs |
https://digitalfire.com/4sight/datasheets/BurgessKaolin.pdf
Burgess Kaolin Data Sheet |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| GE Brightness | 85-92% |
|---|---|
| % Passing 325 Mesh Wet | 99.95+% |
| Particle Shape (1-7 microns) | Thin flat plate |
| Density (Specific Gravity) | 2.63 |
| Moisture Content - Powder | 0.25-0.5% |
| Median Particle Size (Microns) | 1.4 microns |
| pH for dry powder | 5.5 |