Alternate Names: SHMP, Calgon
Description: Deflocculant
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Tetrasodium Pyrophosphate
|
| Typecodes |
Additives for Ceramic Glazes
Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives. |
| URLs |
http://en.wikipedia.org/wiki/Sodium_hexametaphosphate
Sodium Hexametaphosphate at Wikipedia |