Ferro Frit R-1

Description: Bonding frit

Related Information

Links

Oxide Analysis Formula Tolerance
Materials General Frit GF-141
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Bonding Frits
Also called glass frits, these melt at very low temperatures (e.g. 500C). They are used to bond together materials that can withstand some heat (e.g. abrasives, ceramics, non-oxide ceramics, metals). And as a surface-smoothing agent. The main product properties are melting temperature and thermal expansion. The powders are mixed with binders, applied and then heated up and down to create the bond.