Description: Medium lead zinc frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 2.09% | 0.08 | |
| CaO | 5.11% | 0.23 | |
| ZnO | 8.29% | 0.25 | |
| PbO | 38.65% | 0.43 | |
| Al2O3 | 5.46% | 0.13 | |
| B2O3 | 7.92% | 0.28 | |
| SiO2 | 32.48% | 1.35 | |
| Oxide Weight | 250.12 | ||
| Formula Weight | 250.12 | ||
| Materials |
Ferro Frit 3541
|
| Materials |
Pemco Frit Pb-967
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.5 x 10-6 (50-450C) |
|---|---|
| Frit Softening Point | 1550F |