Digitalfire will shut down on June 26. I no longer have the authority to grant exemption to a section in the Terms and Conditions of using material in the Insight-Live account from which I built the source material. While there are ways to comply with the take-down order, they are beyond my means because of how complex and large the site has become in the past 35+ years. It has been a wild ride for a shy prairie boy, thanks to everyone for your support. Insight-live.com is not affected by this.
Alternate Names: Indian Red
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 17.70% | 2.56 | |
| Al2O3 | 4.00% | 0.34 | |
| Fe2O3 | 65.40% | 3.56 | |
| TiO2 | 0.09% | 0.01 | |
| CaO | 3.47% | 0.54 | |
| MgO | 0.05% | 0.01 | |
| Na2O | 2.07% | 0.29 | |
| K2O | 0.74% | 0.07 | |
| P2O5 | 1.50% | 0.09 | |
| LOI | 4.96% | n/a | |
| Oxide Weight | 826.92 | ||
| Formula Weight | 870.08 | ||
Natural red iron oxide is delivered as a red powder or in lump form. It is used in paint, rubber and ceramics.
The analysis given here is only an example, this is a natural material and of course the chemistry is widely variable from place to place. SO3 can be present in significant amounts. Iron content will vary from 40 to 70% and grades are sold according to its amount. Here is another example:
CaO: 0.90
Na2O: 0.80
Al2O3: 1.34
SiO2: 18.32
SO3: 1.97
L.O.I: 2.10
Fe2O3: 64.00

This picture has its own page with more detail, click here to see it.
Natural Red Iron Oxide powder
| Materials |
Iron Oxide Black
|
| Materials |
YLO-1888D Yellow Iron Oxide
|
| Materials |
Iron Oxide Yellow
|
| Materials |
Iron Oxide Red
Red iron oxide is the most common colorant used in ceramic bodies and glazes. As a powder, it is available in red, yellow, black and other colors. |
| Hazards |
Iron oxide and Hematite
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk