USAKOS Wollastonite

Oxide Analysis Formula Tolerance
CaO 46.00% 0.99
SiO2 53.00% 1.06
Fe2O3 0.15% -
Al2O3 0.20% -
MgO 0.20% 0.01
P2O5 0.05% -
Na2O 0.15% -
K2O 0.05% -
TiO2 0.13% -
LOI 1.85%n/a
Oxide Weight 120.65
Formula Weight 122.93

Notes

Hardness 4.5
PH 9.9
Moisture content 0.02%
Sintering temperature 991-1196=B0C
Melting point 1540=B0C
Coefficient of expansion 6.5 x 10-6 cm/cm/=B0C
Water solubility 0.0095g/100.c.c
Aspect ration 2:1
Particle size distribution depends on the size that the product is milled to.

Related Information

Links

Materials Wollastonite
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy