FSC 2.1 Spodumene

Description: Fine Spodumene Concentrate

Oxide Analysis Formula Tolerance
Li2O 7.40% 0.97
K2O 0.20% 0.01
Na2O 0.20% 0.01
Al2O3 26.50% 1.02
SiO2 64.50% 4.20
Fe2O3 0.10% -
P2O5 0.25% 0.01
LOI 0.20%n/a
Oxide Weight 388.16
Formula Weight 388.94

Related Information

Links

URLs http://www.amalgamet.com/Products/minerals.htm
Description of material
Materials Spodumene Concentrate
Materials Foote Spodumene
Materials Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O.
Materials Australian Spodumene

Data

Hardness (Moh) 6-5-7
Frit Softening Point 1420C
Sieve Analysis Dry Tyler 115mesh: 0.5% 200 mesh: 92%
Density (Specific Gravity) 3.2

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy