Description: Tennessee Ball Clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.30% | 0.02 | |
| K2O | 1.20% | 0.05 | |
| MgO | 0.30% | 0.03 | |
| Na2O | 0.20% | 0.01 | |
| TiO2 | 1.50% | 0.07 | |
| Al2O3 | 28.10% | 1.00 | |
| SiO2 | 57.40% | 3.47 | |
| Fe2O3 | 0.80% | 0.02 | |
| LOI | 10.20% | n/a | |
| Oxide Weight | 325.96 | ||
| Formula Weight | 362.99 | ||
This is sold by Chemical Distributors Inc. to be used in a 50:50 mix with Texas Pioneer Talc.
It is a mixture of 75% SGP Ball Clay and 25% OM#4 Ball Clay.
| Materials |
Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries. |
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |