Tetrasodium Pyrophosphate Hydrated

Description: Powerful deflocculant

Oxide Analysis Formula Tolerance
Na2O 27.80% 0.67
P2O5 31.84% 0.33
H2O 40.36%n/a
Oxide Weight 88.65
Formula Weight 148.64

Related Information

Links

Materials Tetrasodium Pyrophosphate
Typecodes Additives for Ceramic Glazes
Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives.
Oxides P2O5 - Phosphorus Pentoxide