Description: Calcium Borate Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 26.61% | 0.98 | |
| K2O | 0.45% | 0.01 | |
| MgO | 0.19% | 0.01 | |
| B2O3 | 50.01% | 1.49 | |
| Al2O3 | 4.89% | 0.10 | |
| SiO2 | 17.85% | 0.61 | |
| Oxide Weight | 206.68 | ||
| Formula Weight | 206.68 | ||
Chemistry similar to colemanite
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron). |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |