Pyrophyl R-1403

Description: Pyrophyllite

Oxide Analysis Formula Tolerance
Na2O 0.20% 0.02
TiO2 0.40% 0.02
Al2O3 21.00% 1.00
SiO2 74.70% 6.04
Fe2O3 0.70% 0.02
K2O 0.20% 0.01
LOI 2.80%n/a
Oxide Weight 472.11
Formula Weight 485.71

Notes

The PYROPHYL group of mineral products consists of milled co-products of the Andafrac series and various milled combinations of the Pyrofrac and Andafrac series. The broad range of alumina contents allows for both whiteware and refractory applications.

Pyrophyl is a high melting material and is used to reduce hot load deformation and improve volume stability in refractories.

Related Information

Links

Materials Pyrophyl R-2252
Materials Pyrophyl R-2253
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Pyrophyl
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Bulk Density lbs/cu. ft. (Packed) 60
Pyrometric Cone Equivalent 29
Sieve Analysis Dry +200 mesh: 12%
Density (Specific Gravity) 2.70

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy