Primas FA-200 Feldspar

Oxide Analysis Formula Tolerance
CaO 0.40% 0.04
K2O 5.89% 0.37
Na2O 6.20% 0.59
TiO2 0.08% 0.01
Al2O3 18.49% 1.07
SiO2 68.47% 6.72
Fe2O3 0.27% 0.01
LOI 0.20%n/a
Oxide Weight 588.25
Formula Weight 589.43

Notes

When substituting this for other feldspars, like Minspar, Custer or G200 HP note that the iron content in this one is quite a bit more. So colors could be different.

Related Information

Links

Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy