Description: Dark Plastic Fire Clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 45.70% | 2.49 | |
| Al2O3 | 31.10% | 1.00 | |
| Fe2O3 | 6.10% | 0.13 | |
| MgO | 0.23% | 0.02 | |
| Na2O | 0.03% | - | |
| K2O | 0.11% | - | |
| CaO | 0.02% | - | |
| TiO2 | 1.70% | 0.07 | |
| LOI | 15.30% | n/a | |
| Oxide Weight | 278.75 | ||
| Formula Weight | 329.10 | ||
Was used up until the 1970s but has not been available since. This material was popular since it fired to a very warm brown in oxidation and deep brown in reduction.

This picture has its own page with more detail, click here to see it.
Cone 10 reduction (top), cone 10 down to 6 oxidation below that (top to bottom). A refractory material.
| Materials |
Fireclay
|
| Typecodes |
Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more. |