Zinc Zircon Silicate

Alternate Names: Zinc Zirconium Silicate

Description: Zirconium Opacifier With Flux

Formula: O9Si3ZnZr

Oxide Analysis Formula Tolerance
ZnO 30.52% 1.00
ZrO2 45.78% 0.99
SiO2 23.08% 1.02
Oxide Weight 265.06
Formula Weight 265.06

Related Information

Links

Typecodes Opacifier
Opacifiers are powders that turn transparent glazes opaque by various chemical and physical mechanisms (and combinations of mechanisms).