Zinc Carbonate

Alternate Names: Smithsonite, zinc spar

Formula: ZnCO3

Oxide Analysis Formula Tolerance
ZnO 64.91% 1.00
CO2 35.09%n/a
Oxide Weight 81.40
Formula Weight 125.40

Related Information

Links

Materials Zinc Oxide
A pure source of ZnO for ceramic glazes, it is 100% pure with no LOI.
Hazards Zinc Compounds Toxicology
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
URLs http://en.wikipedia.org/wiki/Zinc_carbonate
Zinc carbonate at Wikipedia

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy