Torrecid Frit MBK00020

Description: Calcium zinc zircon zero boron matte frit

Oxide Analysis Formula Tolerance
ZnO 4.38% 0.14
Al2O3 18.56% 0.47
ZrO2 9.50% 0.20
MgO 2.12% 0.13
Na2O 2.08% 0.09
SiO2 46.56% 1.98
K2O 2.69% 0.07
Fe2O3 0.13% -
CaO 12.46% 0.57
TiO2 1.39% 0.04
LOI 3.34%n/a
Oxide Weight 255.67
Formula Weight 264.50

Notes

Soft surface, high opacity. Used for the new decoration technology: Inkjet

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy